MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Thermal Ceramics Kaocrete 249 C Low Cement Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kaocrete 249C is a low cement castable designed for internal or external high frequency vibration placement. It provides excellent volume stability and load bearing characteristics for continuous operation of 2800°F (1538°C).

Features:

  • High-strength low cement castables
  • Closely controlled grain sizing
  • Rival the low porosity and low hot load deformation of many dense firebricks
  • Applications:

  • Forge furnace hearths
  • Door jambs
  • Lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and dams
  • Rotary hearth curbs
  • Walking beam furnace hearth
  • Pusher furnace hearths
  • Skid pipe protection
  • Troughs for molten copper
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 2.16 - 2.29 g/cc0.0780 - 0.0827 lb/in³Fired
    Porosity 16 %16 %Fired at 2800°F; ASTM C20
    Deformation 1.9 %1.9 %load-25 psi, 1.5 hours at 2640°F; ASTM C16
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00552 - 0.00827 GPa0.800 - 1.20 ksiDried 18-24 hours at 220°F; ASTM C133
     0.00207 - 0.00345 GPa
    @Temperature 1370 °C
    0.300 - 0.500 ksi
    @Temperature 2500 °F
    ASTM C133
     0.00552 - 0.00827 GPa
    @Temperature 1230 °C
    0.800 - 1.20 ksi
    @Temperature 2250 °F
    ASTM C133
     0.00758 - 0.0110 GPa
    @Temperature 1090 °C
    1.10 - 1.60 ksi
    @Temperature 2000 °F
    ASTM C133
     0.00896 - 0.0117 GPa
    @Temperature 816 °C
    1.30 - 1.70 ksi
    @Temperature 1500 °F
    ASTM C133
     0.00552 - 0.00896 GPa
    @Treatment Temp. 816 °C,
    Time 18000 sec
    0.800 - 1.30 ksi
    @Treatment Temp. 1500 °F,
    Time 5.00 hour
    ASTM C133
     0.0110 - 0.0159 GPa
    @Treatment Temp. 1540 °C,
    Time 18000 sec
    1.60 - 2.30 ksi
    @Treatment Temp. 2800 °F,
    Time 5.00 hour
    ASTM C133
    Compressive Strength 41.0 - 62.0 MPa5950 - 8990 psiDried for 18-24 hours at 220°F
     48.0 - 76.0 MPa6960 - 11000 psiFired 5 hours at 1500°F; ASTM C133
     41.0 - 90.0 MPa5950 - 13100 psiFired 5 hours at 2800°F
    Abrasion 8.0 - 128.0 - 12loss, cc`s; Fired 5 hours at 1500°F; ASTM C704
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  1.43 W/m-K
    @Temperature 260 °C
    9.90 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C417
     1.50 W/m-K
    @Temperature 538 °C
    10.4 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C417
     1.57 W/m-K
    @Temperature 816 °C
    10.9 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C417
     1.63 W/m-K
    @Temperature 1090 °C
    11.3 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C417
    Maximum Service Temperature, Air 1540 °C2800 °F
    Shrinkage  0.10 - 0.40 %
    @Temperature 816 °C,
    Time 18000 sec
    0.10 - 0.40 %
    @Temperature 1500 °F,
    Time 5.00 hour
    ASTM C113
     0.20 - 0.60 %
    @Temperature 1540 °C,
    Time 18000 sec
    0.20 - 0.60 %
    @Temperature 2800 °F,
    Time 5.00 hour
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    0.00 - 0.20 %
    @Treatment Temp. 220 °F
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 12.0 Month12.0 Month
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 50 %50 %
    Alkalis 0.10 %0.10 %
    CaO 1.9 %1.9 %
    Fe2O3 0.80 %0.80 %
    MgO 0.10 %0.10 %
    SiO2 46 %46 %
    TiO2 1.5 %1.5 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC
    Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
    China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
    Chosun Refractories AB10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
    Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom

    CTHERM071 / 2391

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.