MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kaocrete 249 C Low Cement Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kaocrete 249C is a low cement castable designed for internal or external high frequency vibration placement. It provides excellent volume stability and load bearing characteristics for continuous operation of 2800°F (1538°C).

Features:

  • High-strength low cement castables
  • Closely controlled grain sizing
  • Rival the low porosity and low hot load deformation of many dense firebricks
  • Applications:

  • Forge furnace hearths
  • Door jambs
  • Lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and dams
  • Rotary hearth curbs
  • Walking beam furnace hearth
  • Pusher furnace hearths
  • Skid pipe protection
  • Troughs for molten copper
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 2.16 - 2.29 g/ccFired
    Porosity 16 %Fired at 2800°F; ASTM C20
    Deformation 1.9 %load-25 psi, 1.5 hours at 2640°F; ASTM C16
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.800 - 1.20 ksiDried 18-24 hours at 220°F; ASTM C133
     0.300 - 0.500 ksi
    @Temperature 1370 °C
    ASTM C133
     0.800 - 1.20 ksi
    @Temperature 1230 °C
    ASTM C133
     1.10 - 1.60 ksi
    @Temperature 1090 °C
    ASTM C133
     1.30 - 1.70 ksi
    @Temperature 816 °C
    ASTM C133
     0.800 - 1.30 ksi
    @Treatment Temp. 816 °C,
    Time 18000 sec
    ASTM C133
     1.60 - 2.30 ksi
    @Treatment Temp. 1540 °C,
    Time 18000 sec
    ASTM C133
    Compressive Strength 41.0 - 62.0 MPaDried for 18-24 hours at 220°F
     48.0 - 76.0 MPaFired 5 hours at 1500°F; ASTM C133
     41.0 - 90.0 MPaFired 5 hours at 2800°F
    Abrasion 8.0 - 12loss, cc`s; Fired 5 hours at 1500°F; ASTM C704
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 9.90 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    ASTM C417
     10.4 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    ASTM C417
     10.9 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    ASTM C417
     11.3 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    ASTM C417
    Maximum Service Temperature, Air 2800 °F
    Shrinkage 0.10 - 0.40 %
    @Temperature 816 °C,
    Time 18000 sec
    ASTM C113
     0.20 - 0.60 %
    @Temperature 1540 °C,
    Time 18000 sec
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesOriginal ValueComments
    Shelf Life 12.0 Month
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 50 %
    Alkalis 0.10 %
    CaO 1.9 %
    Fe2O3 0.80 %
    MgO 0.10 %
    SiO2 46 %
    TiO2 1.5 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC
    Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
    China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
    Chosun Refractories AB10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
    Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom

    CTHERM071 / 2391

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.