MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hytrel® HTR4275 BK316 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Melt Density 1.00 g/cc
@Temperature 240 °C
Water Absorption 0.50 %
@Time 86400 sec
Immersion; Sim. to ISO 62
 0.50 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.017 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cmISO 294-4, 2577
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
cm³/10min Volumetric; ISO 1133
 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5215s; ISO 48-4
 <= 55ISO 48-4
Tensile Stress at Strain 6.70 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 10.4 MPa
@Strain 10 %
ISO 527-1/-2
 17.0 MPa
@Strain 50 %
ISO 527-1/-2
 21.0 MPa
@Strain 100 %
ISO 527-1/-2
Tensile Modulus 160 MPaISO 527-1/-2
Flexural Modulus 160 MPaISO 178
Poissons Ratio 0.49
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 160 kJ/m²
@Temperature -30.0 °C
Partial Break; ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Tensile Impact Strength 410 kJ/m²
@Temperature 23.0 °C
Notched; ISO 8256/1
Tensile Creep Modulus, 1 hour 140 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 90.0 MPa1000h; ISO 899-1
Tear Strength 127 kN/mnormal; ISO 34-1
 140 kN/mparallel; ISO 34-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 181 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 185 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 2.10 J/g-°C
@Temperature 240 °C
Melt
Thermal Conductivity 0.150 W/m-K
@Temperature 240 °C
Melt
Melting Point 192 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °CISO 75-1/-2
Brittleness Temperature -100 °CISO 974
Glass Transition Temp, Tg -30.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
Flame Spread 38.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 - 220 °CRange, Extrusion
 220 - 240 °CRange, Blow Molding
 230 °COptimum, Blow Molding
 240 °COptimum, Injection
 230 - 250 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 40.0 - 50.0 °CInjection
 40.0 - 90.0 °CRange, Blow Molding
 80.0 °COptimum, Blow Molding
Drying Temperature 100 °CInjection
 100 °CExtrusion
 100 - 110 °CBlow Molding
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hourBlow Molding, Dehumidified Dryer
Moisture Content <= 0.030 %Blow Molding
 <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesBlow Molding
 yesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
FMVSS ClassBISO 3795 (FMVSS 302)
Odor Class3.5VDA 270
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® BM70G20HSLX BK537 PA66-IGF20
Celanese Hytrel® 21UV TPC-ET
Celanese Hytrel® 30HS PA+TPC-ET
Celanese Hytrel® 3078 TPC-ET
Celanese Hytrel® HTR8206 TPC-ET

PDSX5203 / 197843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.