MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® IP 4520 General Purpose Molding
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4520 is an amorphous EPDM grade designed for molded applications. It is ideally suited for injection and transfer molded brake parts, corner moldings, general purpose gaskets and moldings. The combination of low viscosity and low crystallinity allows for good processability, low temperature properties and performance without the addition of a plasticizer.

Information provided by manufacturer.

Key Words: 0822A32-03
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.156 g/cc
Mooney Viscosity 33
@Temperature 100 °C
ML 1 + 4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 7.60 MPaVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 460 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00260 GPa
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00470 GPa
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00600 GPa
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 31.8 kN/mDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 81 %
@Temperature 125 °C
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -41.0 °CTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5TMQ
 0.5Sulfur
 0.75TMTD
 0.75DPTT
 1.5ZnDBC
 1.5MBT
 100Nordel® IP 4520
 125N774 Black
 5Zinc Oxide
 50Paraffinic Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound
Dow Nordel® IP 4570 Radiator/Heater Hose
Dow Nordel® IP 4520 General Purpose Compound
Dow Nordel® IP 4520 Molded Brake Part
Dow Nordel® IP 4520 Molded Golf Grip

PDVG10 / 34130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.