MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman AP006 Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Automotive components
  • Breathable films
  • Electrical/electronic components
  • Film Modification
  • Flexible hinges
  • Hose mandrel
  • Industrial components
  • Industrial hoses/belts
  • Office furniture
  • Packaging
  • Polymer modification
  • Profiles
  • Rubber and plastic modification
  • Sporting goods
  • Thermoplastic elastomer compounds
  • Tubing

Key Attributes:

  • Environmentally preferred, non-halogenated material
  • Excellent chemical and oil resistance
  • Excellent compatibility with a wide range of polymers
  • Excellent processability
  • Exceptional heat resistance and high temperature dimensional stability
  • High energy absorption
  • High flexibility without plasticizers
  • Melt bondable to a variety of substrates, including PVC
  • Outstanding toughness and puncture resistance
  • Solvent bondable

Product Description: Eastman AP006 is a tough, clear, durable copolyester ether that combines the strength of plastics, the flexibility of elastomers, and the processability of thermoplastics. Eastman AP006 can be used in injection molding and film or tubing extrusion applications or in any application that demands strength, durability, chemical resistance, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, high temperature resistance and flexibility without the addition of plasticizers. Eastman AP006 is considered environmentally preferred because of its non-halogenated material composition. Its broad compatibility with other polymers such as styrenic block copolymers makes it an excellent choice for both alloys and as additives/modifiers to improve performance properties.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 0.40 %
@Time 86400 sec
Immersion; ASTM D570
Viscosity Measurement 1.16Inherent; EMN-A-AC-G-V-1
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Hardness, Shore D 55ASTM D2240
Tensile Strength at Break 22.0 MPaASTM D638
Tensile Strength, Yield 14.0 MPaASTM D638
Elongation at Break 400 %ASTM D638
Elongation at Yield 38 %ASTM D638
Tensile Modulus 170 MPaASTM D638
Flexural Modulus 150 MPaASTM D790
Izod Impact, Notched 40.0 J/m
@Temperature -40.0 °C
ASTM D256
Tear Strength, Total 350 NASTM D1004
Torsional Stiffness 240 MPa
@Temperature -28.0 °C
ASTM D1043
 930 MPa
@Temperature <=-70.0 °C
ASTM D1043
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 27.0 J/gASTM E793
CTE, linear 150 µm/m-°CASTM D696
Specific Heat Capacity 1.60 J/g-°C
@Temperature 25.0 °C
solid; DSC
 1.80 J/g-°C
@Temperature 100 °C
solid; DSC
 2.00 J/g-°C
@Temperature 150 °C
solid; DSC
 2.30 J/g-°C
@Temperature 175 °C
solid; DSC
 2.30 J/g-°C
@Temperature 225 °C
melt; DSC
 3.10 J/g-°C
@Temperature 200 °C
transition; DSC
Thermal Conductivity 0.190 W/m-KASTM C177
Melting Point 205 °CCrystalline Peak; ASTM D3418
Crystallization Temperature 140 °CDSC
Vicat Softening Point 170 °C
@Load 1.00 kg
ASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
Glass Transition Temp, Tg -3.00 °CDSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman AP005 Copolyester
Telles Bio-based Natural Plastics™ Aliphatic Copolyester, for Extruded Cast Film and Sheet
Eastman Neostar FN005 Elastomer
Eastman AP007 Copolyester
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release

PE8813 / 129658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.