MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zenite® FG7145L BK011 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: Zenite® FG7145L BK011 is a 45% glass reinforced, lubricated liquid crystal polymer resin with FDA approval for use in repeated food-contact applications.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccISO 1183
Filler Content 45 %
Linear Mold Shrinkage, Flow 0.00050 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 527
 130 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
ISO 527
 140 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
ISO 527
Elongation at Break 0.60 %
@Thickness 1.00 mm,
Temperature 23.0 °C
ISO 527
 0.90 %
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 527
 0.90 %
@Thickness 2.00 mm,
Temperature 23.0 °C
ISO 527
Tensile Modulus 18000 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 527
 20500 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
ISO 527
 22000 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
ISO 527
Flexural Strength 180 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 178
 210 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
ISO 178
 230 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
ISO 178
Flexural Modulus 17500 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 178
 20500 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
ISO 178
 24000 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
ISO 178
Charpy Impact Unnotched 1.80 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 352 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 295 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 365 °COptimum
 360 - 370 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericLCP
Part Marking Code>LCP-GF45<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryFood Contact Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zenite® 5145L BK010 LCP
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese Zenite® 6635 BK010 LCP
Celanese Zenite® 7130 BK010 LCP (Extended Tabular Temperature Data)

PDTA7790 / 89727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.