MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.

CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting according to DIN EN 13432.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccISO 1183
Moisture Absorption 0.500 %
@Temperature 23.0 °C
normal humidity; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 105 MPaISO 2039-1
Tensile Strength 22.7 MPa5 mm/min; ISO 527-2
Elongation at Break 11.8 %ISO 527-2
Tensile Modulus 2740 MPaISO 527-2
Flexural Modulus 1820 MPaISO 178
Charpy Impact Unnotched 58.0 kJ/m²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 152 °CDSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 40.0 °Ccontinuous
 58.0 °Cshort term
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °CISO 75-2
Vicat Softening Point 58.0 °CVST/B/50; ISO 306
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Compliance
 
Descriptive Properties
ColorWhite
Food Compliance BfR:Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baypreg® F Polyurethane, Natural Fiber Glass
CENTROPLAST BC Organic Thermoplastic
Covestro Desmomelt® 540/2 Polyurethane
Covestro Desmomelt® 540/1 Polyurethane
Covestro Desmomelt® 530 Polyurethane

PCENTR46 / 150232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.