MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Available in: Asia Pacific, Europe and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183/A
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 20 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
shear rate: 1000/s
 20 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
shear rate: 1000/s
 20 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
shear rate: 1000/s
 170 cP
@Shear Rate 100 1/s,
Temperature 300 °C
shear rate: 100/s
 180 cP
@Shear Rate 100 1/s,
Temperature 290 °C
shear rate: 100/s
 190 cP
@Shear Rate 100 1/s,
Temperature 280 °C
shear rate: 100/s
 320 cP
@Shear Rate 10 1/s,
Temperature 300 °C
shear rate: 10/s
 400 cP
@Shear Rate 10 1/s,
Temperature 290 °C
shear rate: 10/s
 450 cP
@Shear Rate 10 1/s,
Temperature 280 °C
shear rate: 10/s
Linear Mold Shrinkage 0.0055 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0044 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 220 MPaASTM D638
 240 MPaISO 527 Type 1A
Tensile Stress at Strain 155 MPa
@Strain 1 %
 240 MPa
@Strain 2 %
Elongation at Break 2.0 %ASTM D638
Tensile Modulus 16200 MPaISO 527 Type 1A
Flexural Strength 350 MPaASTM D790
Flexural Modulus 13500 MPaISO 178
 13800 MPaASTM D790
Izod Impact, Notched 180 J/mASTM D256
Izod Impact, Notched (ISO) 14.5 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 95.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 16.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
1210
 HB
@Thickness 1.60 mm
1210
 HB
@Thickness 3.20 mm
1210
Oxygen Index 23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 0.800 mm
ISO 60695-2-12
 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 700 °C
@Thickness 3.20 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned
DuPont Mobility and Materials Zytel® 70G35HSL BK039B PA66-GF35
Domo TECHNYL® A 218 V50 Black 21N PA 66 50% Glass Reinforced, Dry
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY

PRHOD653 / 137884

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.