MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3462 Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Homopolymer extrusion grade for slit film and fibrillated tapes

Process Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.

FDA - FINA 3462 complies with all applicable FDA regulations for food contact applications.

Recommended Applications -- FINA 3462 is recommended for slit film monofilament and fibrillated tape applications requiring improved process stability.

Processing - FINA 3462 processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 4.1 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92ASTM D288A
Hardness, Shore D 80ASTM D1706
Tensile Strength, Ultimate 34.5 MPaASTM D638
Elongation at Break 12 %ASTM D638
Modulus of Elasticity 1.515 GPaASTM D638
Flexural Modulus 1.38 GPaASTM D790
Izod Impact, Notched 0.317 J/cmASTM D256A
Izod Impact, Unnotched 9.00 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 107 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 260 °CExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating
Overview of materials for Polypropylene, Molded
Aclo Accucomp Polypropylene HPO306L Homopolymer
Total PPH 4030 Polypropylene Homopolymer
Total PPC 5720WZ Polypropylene, Impact Copolymer

PFIN16 / 38346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.