MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OJSC Plastic Grade 1 Expanded Polystyrene (EPS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Self-extinguishing, contains a flame retardant. Intended for the manufacturing of blocks, insulation boards. The product is used for the production of thermal/sound insulation and packaging.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.0200 g/ccpacked
Relative Viscosity >= 1.65 cP
Outgassing - Total Mass Loss <= 1.0 %%, during drying
 
Thermal PropertiesOriginal ValueComments
Flammability Test 2.0time shelf, combustion, sec
 
Descriptive Properties
Breaking Stress1.2static blending, kg/cm²
Mass Fraction10%, on a sieve with cell size 1.4mm
 85%, on a sieve with cell size 1.6mm
Mass Fraction of Particles95%, particles of the main fraction
Mass Fraction of Residual Monomer0.2styrene %
Size (mm)2.5
Weight Percent of Blowing Agent7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical R160 EPS, Flame Retardant
LG Chemical B160 EPS, Non-Flame Retardant
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene
Ineos Nova T163B Expandable Polystyrene

POJSC980 / 192489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.