MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zenite® FG7145L BK011 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: Zenite® FG7145L BK011 is a 45% glass reinforced, lubricated liquid crystal polymer resin with FDA approval for use in repeated food-contact applications.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0629 lb/in³ISO 1183
Filler Content 45 %45 %
Linear Mold Shrinkage, Flow 0.00050 cm/cm
@Thickness 2.00 mm
0.00050 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  120 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
17400 psi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527
 130 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
18900 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 527
 140 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
20300 psi
@Thickness 0.0394 in,
Temperature 73.4 °F
ISO 527
Elongation at Break  0.60 %
@Thickness 1.00 mm,
Temperature 23.0 °C
0.60 %
@Thickness 0.0394 in,
Temperature 73.4 °F
ISO 527
 0.90 %
@Thickness 4.00 mm,
Temperature 23.0 °C
0.90 %
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527
 0.90 %
@Thickness 2.00 mm,
Temperature 23.0 °C
0.90 %
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 527
Tensile Modulus  18.0 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
2610 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527
 20.5 GPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2970 ksi
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 527
 22.0 GPa
@Thickness 1.00 mm,
Temperature 23.0 °C
3190 ksi
@Thickness 0.0394 in,
Temperature 73.4 °F
ISO 527
Flexural Strength  180 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
26100 psi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 178
 210 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
30500 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 178
 230 MPa
@Thickness 1.00 mm,
Temperature 23.0 °C
33400 psi
@Thickness 0.0394 in,
Temperature 73.4 °F
ISO 178
Flexural Modulus  17.5 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
2540 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 178
 20.5 GPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2970 ksi
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 178
 24.0 GPa
@Thickness 1.00 mm,
Temperature 23.0 °C
3480 ksi
@Thickness 0.0394 in,
Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 352 °C666 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 295 °C563 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 365 °C689 °FOptimum
 360 - 370 °C680 - 698 °F
Mold Temperature 80.0 °C176 °FOptimum
 40.0 - 150 °C104 - 302 °F
Drying Temperature 150 °C302 °F
Dry Time 3 hour3 hourDehumidified Dryer
Moisture Content <= 0.010 %<= 0.010 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericLCP
Part Marking Code>LCP-GF45<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryFood Contact Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 5145L BK010 LCP
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese Zenite® 6635 BK010 LCP
Celanese Zenite® 7130 BK010 LCP (Extended Tabular Temperature Data)

PDTA7790 / 89727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.