System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Lubrizol LifeSciences Tecophilic® HP-60D-60 Hydrophilic TPU – Extrusion Grade
Lubrizol LifeSciences Tecophilic® HP-93A-100 Hydrophilic TPU – Extrusion Grade
Lubrizol LifeSciences Tecophilic® SP-60D-60 Solution Grade Hydrophilic TPU
Lubrizol LifeSciences Tecophilic® SP-80A-150 Solution Grade Hydrophilic TPU
Lubrizol LifeSciences Tecophilic® SP-93A-100 Solution Grade Hydrophilic TPU
Lubrizol LifeSciences Tecophilic® TG-2000 Hydrophilic TPU Hydrogel
Lubrizol LifeSciences Tecophilic® TG-500 Hydrophilic TPU Hydrogel
Lubrizol LifeSciences Tecoplast® Series OP-770/Opaque Resins TPU
Lubrizol LifeSciences Tecoplast® Series TP-470/Clear Resins TPU
Lubrizol LifeSciences Tecothane® 58092 NAT 028 TPU
Lubrizol LifeSciences Tecothane® Soft AR-62A TPU
Lubrizol LifeSciences Tecothane® Soft AR-75A TPU
Lubrizol LifeSciences Tecothane® Soft AR-85A TPU
Lubrizol LifeSciences Tecothane® Soft AR-95A TPU
Lubrizol LifeSciences Tecothane® TT-1055D TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1065D TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1069D TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1072D TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1074A TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1075D-M TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1085A TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1095A TPU - Clear
Lubrizol LifeSciences Tecothane® TT-2055D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2055D-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2065D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2065D-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2069D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2072D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2074A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2074A-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2075D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2075D-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2085A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2085A-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2095A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2095A-B40 TPU – 40% Barium Sulfate
Lubrizol Pearlbond® UB410B Thermoplastic Polyurethane
Lubrizol Pearlbond™ 1160L Polyurethane
Lubrizol Pearlbond™ 220 Polyurethane
Lubrizol Pearlbond™ 223 Polyurethane
Lubrizol Pearlbond™ 301 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 302 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 305 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 360 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 5713 F1 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 5717 NT2 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 700 EXP Thermoplastic Polyurethane
Lubrizol Pearlbond™ 700 HMS EXP Thermoplastic Polyurethane
Lubrizol Pearlbond™ 702 EXP Thermoplastic Polyurethane
Lubrizol Pearlbond™ 920 Thermoplastic Polyurethane
Lubrizol Pearlbond™ 960 EXP Thermoplastic Polyurethane
Lubrizol PEARLBOND™ UB410A Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-50/14 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-50/29 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-60/03SP Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-60/18SP Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-60/21 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-60/25SP Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 45-60/34 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 5701 F51 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5701 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 5702 F3 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5703 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5707 F1 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 5707 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5708 F4 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5712 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5713 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5714 Thermoplastic Polyurethane
Lubrizol PEARLSTICK™ 5715 F2 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5715 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5719 Thermoplastic Polyurethane
Lubrizol Pearlstick™ 5778 Thermoplastic Polyurethane
Lubrizol Pearlthane™ ECO D12T80E Thermoplastic Polyurethane
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Lubrizol Stat-Rite® M-809 Static Control Acrylic
Lubrizol Stat-Rite® S-102 Static Control Polypropylene
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Lubrizol Stat-Rite® S-250 Static Control Polypropylene
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy
Lubrizol Stat-Rite® SIS535 Static Control System
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene
Lubrizol STAT-RITE® X-5091 Ether-Type Static Dissipative Polymer
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound
Lubrizol Telene 1610 A/B & A/BK Dicyclopentadiene (DCPD)
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD)
Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD)
Lubrizol Thermedics™ Carbothane™ PC-3585A-B40 Polycarbonate-based Polyurethane Biomedical Elastomer
Lucas-Milhaupt 40SN/60PB General Purpose Tin/Lead Solder (ASTM B32 Sn40A)
Lucas-Milhaupt 50/50 General Purpose Tin/Lead Solder
Lucas-Milhaupt 60/40 Tin-Lead Soft Solder (ASTM B32 Sn60)
Lucas-Milhaupt 60-112 Copper Filler Metal (AWS BCu-1a)
Lucas-Milhaupt 63/37 63 Sn / 37 Pb Tin-Lead Soft Solder (ASTM B32 Sn63)
Lucas-Milhaupt 69-270 Titanium Bearing active Metal Alloy
Lucas-Milhaupt 69-273 Titanium Joining Alloy
Lucas-Milhaupt 80AU/20SN Gold Tin Eutectic Solder
Lucas-Milhaupt 97.5/ 1.5 / 1 (97.5 Pb / 1.5 Ag / 1 Sn) Lead-Silver-Tin Soft Solder (ASTM B32 Ag 1.5)
Lucas-Milhaupt 97.5/ 2.5 (97.5 Pb / 2.5 Ag) Lead-Silver Soft Solder (ASTM B32 Ag 2.5)
Lucas-Milhaupt AL 716 Aluminum Brazing Filler Metal
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Lucas-Milhaupt AL 719 Aluminum Brazing Filler Metal
Lucas-Milhaupt AL 802 Aluminum Brazing Filler Metal
Lucas-Milhaupt AL 815 Aluminum Brazing Filler Metal
Lucas-Milhaupt AL 822 Al/Zn Braze Alloy
Lucas-Milhaupt Black Flux Silver Brazing Flux
Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 380
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 604 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Lucas-Milhaupt CDA 101 Certified OFHC (Oxygen Free High Conductivity Copper) (ASTM B170 Grade 1)
Lucas-Milhaupt CDA 102 Oxygen Free Copper, UNS C10200 (AWS BCu-3)
Lucas-Milhaupt CDA 110 Electrolytic Tough Pitch Copper (AWS BCu-1b)
Lucas-Milhaupt CDA 521 Copper Tin Brazing Alloy
Lucas-Milhaupt CDA 681 Low Fuming Bronze Filler Metal
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
Lucas-Milhaupt Cerametil 721 Active Metal Brazing
Lucas-Milhaupt Clean & Bright 5 Tin/ Silver Solder
Lucas-Milhaupt Clean & Bright 6 Tin/ Silver Solder
Lucas-Milhaupt Clean & Bright Tin/ Silver Solder
Lucas-Milhaupt Clean ‘n Brite™ 95/5 Tin Solder Alloy (ASTM B32 Sb5)
Lucas-Milhaupt Dispensable Flux
Lucas-Milhaupt Dry Flux Silver Brazing Flux
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal
Lucas-Milhaupt EASY FLO 35 Silver Based Cadmium-Bearing Filler Metal
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Lucas-Milhaupt Easy-Flo 053 (TEC) Silver Based Cadmium-Bearing Filler Metal
Lucas-Milhaupt Easy-Flo 25 Brazing Alloy
Lucas-Milhaupt EASY-FLO® 056 (BRAZE™ 056) Cadmium Solder/Braze Alloy
Lucas-Milhaupt EASY-FLO® 44 (BRAZE™ 440, SILVALOY® 44) Low Melting Filler Metal
Lucas-Milhaupt EASY-FLO® SILVALOY® 50 General Purpose Braze Filler Metal (AWS BAg-1a)
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal
Lucas-Milhaupt FOS FLO 7 Copper Phosphorus Alloy (AWS BCuP-2)
Lucas-Milhaupt HANDY FLO 100 Series General Purpose flux Binders
Lucas-Milhaupt HANDY FLO 200 Series Flux Binders
Lucas-Milhaupt HANDY FLO 300 Series Flux-free Brazing Binders
Lucas-Milhaupt HANDY FLO 400 Series Flux-free Brazing Binders
Lucas-Milhaupt HANDY FLO 500 Series Brazing Binders
Lucas-Milhaupt HANDY FLO 600 Series Furnace Braze Flux-free Binders
Lucas-Milhaupt HANDY FLO 700 Series Flux Binders
Lucas-Milhaupt HANDY FLO 800 Series Flux Binders
Lucas-Milhaupt HANDY FLO® 6 (SILVALOY® 6, SILVALOY® 6 EXCEL, SIL-FOS® 6M) Copper Braze Alloy
Lucas-Milhaupt HANDY HI-TEMP 095 Carbide Brazing Alloy
Lucas-Milhaupt HANDY HI-TEMP 548® Carbide Brazing Alloy
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy
Lucas-Milhaupt HANDY ONE SILVALOY 505 (HANDY ONE® BRAZE™ 505) Flux Cored Silver Brazing Material (AWS BAg-24)
Lucas-Milhaupt HANDY TYPE TEC Liquid Soldering Flux
Lucas-Milhaupt Handy® Flux B-1 Boron Modified Water Based Fluoride/Borate Flux (AWS A5.31 FB3C)
Lucas-Milhaupt Handy® Flux Hi-Temp Boron Modified Water Based Fluoride/Borate Flux (AWS A5.31 FB3D)
Lucas-Milhaupt Handy® Flux Hi-Temp Water Based Fluoride/Borate Flux (AWS A5.31 FB3D)
Lucas-Milhaupt Handy® Flux Water Based Fluoride/Borate Flux (AWS A5.31 FB3A)
Lucas-Milhaupt HI-TEMP® 095 Copper-Nickel-Manganese Filler Metal
Lucas-Milhaupt HI-TEMP® 548 Nickel Silver Filler Metal
Lucas-Milhaupt HI-TEMP® 720 General-Purpose Nickel Brazing Alloy (AWS BNi-1)
Lucas-Milhaupt HI-TEMP® 820 Nickel-Chromium-Silicon-Boron-Iron Brazing Alloy
Lucas-Milhaupt HI-TEMP® 910 Nickel-Silicon-Boron-Iron Brazing Alloy (AWS BNi-3)
Lucas-Milhaupt HI-TEMP® 930 Nickel-Silicon-Boron-Iron Brazing Alloy (AWS BNi-4)
Lucas-Milhaupt HI-TEMP® 932 Nickel-Phosphorus Brazing Alloy Powder (AWS BNi-6)
Lucas-Milhaupt HI-TEMP® 933 Nickel-Chromium-Phosphorus Brazing Alloy Powder
Lucas-Milhaupt Lithobraze 720 (BT) Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt LM 69-241 Silver Braze Alloy
Lucas-Milhaupt Lucanex 616 Active Metal Brazing
Lucas-Milhaupt Lucanex 716 Active Metal Brazing
Lucas-Milhaupt Lucanex 721 Active Metal Brazing
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy
Lucas-Milhaupt Premabraze 616 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt PREMABRAZE® 127 Gold-Copper Braze Alloy (AWS BAu-3)
Lucas-Milhaupt PREMABRAZE® 140 Gold-Copper Braze Alloy
Lucas-Milhaupt PREMABRAZE® 300 Gold-Nickel Braze Alloy (AWS BAu-5)
Lucas-Milhaupt PREMABRAZE® 399 Gold-Copper Braze Alloy (AWS BAu-1)
Lucas-Milhaupt PREMABRAZE® 402 Gold-Copper Braze Alloy (AWS BVAu-10)
Lucas-Milhaupt PREMABRAZE® 407 Gold-Copper Braze Alloy
Lucas-Milhaupt PREMABRAZE® 408 Gold-Copper Braze Alloy
Lucas-Milhaupt PREMABRAZE® 409 Gold-Copper Braze Alloy
Lucas-Milhaupt PREMABRAZE® 500 Gold-Nickel-Palladium Braze Alloy (AWS BVAu-7)
Lucas-Milhaupt PREMABRAZE® 51 Gold-Copper Braze Alloy
Lucas-Milhaupt PREMABRAZE® 700 Gold-Nickel-Palladium Braze Alloy
Lucas-Milhaupt PREMABRAZE® 800 Gold-Tin Braze Alloy
Lucas-Milhaupt SIL-FOS® 15 Copper-Copper Brazing (Silvaloy® 15 Excel)
Lucas-Milhaupt SIL-FOS® 18 Silver/ Copper/ Phosphorus Alloy
Lucas-Milhaupt SIL-FOS® 2 Silver/ Copper/ Phosphorus Alloy
Lucas-Milhaupt SIL-FOS® 5 Silver/ Copper/ Phosphorus Alloy
Lucas-Milhaupt SIL-FOS® 6 Silver/ Copper/ Phosphorus Alloy
Lucas-Milhaupt SIL-FOS® Silver/ Copper/ Phosphorus Alloy
Lucas-Milhaupt Silvabraze 33830 Brazing Alloy
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder
Lucas-Milhaupt SILVABRITE® 973 High Strength Tin Solder
Lucas-Milhaupt Silvabrite® Lead-Free Solder
Lucas-Milhaupt Silvabrite® S™ Lead-Free Solder
Lucas-Milhaupt SILVABRITE® Zinc Chloride Paste Solder Flux
Lucas-Milhaupt Silvacap 35490 Brazing Alloy
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy
Lucas-Milhaupt Silvacore® A56T Flux Cored Brazing Alloy
Lucas-Milhaupt Silvacote® A50N Brazing Alloy
Lucas-Milhaupt Silvalite Brazing Alloy
Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy
Lucas-Milhaupt Silvaloy® 0 Brazing Alloy
Lucas-Milhaupt Silvaloy® 051 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt SILVALOY® 071 (BRAZE™ 071, SILVALOY® B7T) Copper Silver Tin Brazing Filler Metal
Lucas-Milhaupt SILVALOY® 090 (BRAZE™ 090, SILVALOY® A9) Copper Silver Zinc Brazing Filler Metal
Lucas-Milhaupt Silvaloy® 15 Brazing Alloy
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy
Lucas-Milhaupt SILVALOY® 202 (BRAZE™ 202, SILVALOY® A20) Copper Silver Zinc Braze Alloy
Lucas-Milhaupt Silvaloy® 250 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Silvaloy® 255 Brazing Alloy
Lucas-Milhaupt Silvaloy® 2M Brazing Alloy
Lucas-Milhaupt Silvaloy® 300 Brazing Alloy
Lucas-Milhaupt Silvaloy® 351 Brazing Alloy
Lucas-Milhaupt Silvaloy® 380 Brazing Alloy
Lucas-Milhaupt Silvaloy® 401
Lucas-Milhaupt Silvaloy® 402 Brazing Alloy
Lucas-Milhaupt Silvaloy® 403 Carbide Brazing Alloy
Lucas-Milhaupt SILVALOY® 404 (BRAZE™ 404, SILVALOY® A40N5) Copper Silver Zinc Brazing Filler Metal
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy
Lucas-Milhaupt Silvaloy® 450 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Silvaloy® 452
Lucas-Milhaupt SILVALOY® 452 (Braze™452) Flux Coated Rod (AWS BAg-36)
Lucas-Milhaupt Silvaloy® 495 Carbide Brazing Alloy
Lucas-Milhaupt Silvaloy® 5 Brazing Alloy
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Lucas-Milhaupt Silvaloy® 501 Brazing Alloy
Lucas-Milhaupt SILVALOY® 503 VTG (BRAZE™ 503 VTG & SILVALOY® B50V) Copper Silver Braze Alloy (AWS BVAg-6b Grade 2)
Lucas-Milhaupt SILVALOY® 505 (BRAZE™ 505, SILVALOY® A50N) Silver-Copper Alloy Flux Coated Rod (AWS BAg-24)
Lucas-Milhaupt Silvaloy® 505 Carbide Brazing Alloy
Lucas-Milhaupt Silvaloy® 541 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Silvaloy® 559 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Silvaloy® 560 (Braze™ 560) Silver-Copper-Zinc Alloy (AWS BAg-7)
Lucas-Milhaupt SILVALOY® 560 (Braze™ 560, Silvaloy® A56T FC) Silver-Copper-Zinc Alloy Flux Coated Rod (AWS BAg-7)
Lucas-Milhaupt Silvaloy® 580 Silver Based Cadmium Free Filler Metal
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.