MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zenite® 6330 NC010 LCP (Extended Tabular Temperature Data)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Zenite® 6330 NC010 is a 30% mineral reinforced liquid crystal polymer resin having excellent toughness and a heat deflection temperature of 245°C.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D 792
Density 1.64 g/cc0.0592 lb/in³ISO 1183
Filler Content 30 %30 %
Linear Mold Shrinkage, Flow  0.00 cm/cm
@Thickness 3.17 mm
0.00 in/in
@Thickness 0.125 in
ASTM D955
 0.00 cm/cm
@Thickness 2.00 mm
0.00 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse  0.0050 cm/cm
@Thickness 3.17 mm
0.0050 in/in
@Thickness 0.125 in
ASTM D955
 0.0065 cm/cm
@Thickness 2.00 mm
0.0065 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527
Tensile Strength, Ultimate  48.0 MPa
@Temperature 150 °C
6960 psi
@Temperature 302 °F
ASTM D 638
 56.0 MPa
@Temperature 120 °C
8120 psi
@Temperature 248 °F
ASTM D 638
 125 MPa
@Temperature 23.0 °C
18100 psi
@Temperature 73.4 °F
ASTM D 638
 200 MPa
@Temperature -40.0 °C
29000 psi
@Temperature -40.0 °F
ASTM D 638
Elongation at Break 5.0 %5.0 %ISO 527
 2.5 %
@Temperature 150 °C
2.5 %
@Temperature 302 °F
ASTM D 638
 3.2 %
@Temperature 120 °C
3.2 %
@Temperature 248 °F
ASTM D 638
 4.0 %
@Temperature 23.0 °C
4.0 %
@Temperature 73.4 °F
ASTM D 638
Tensile Modulus  4.80 GPa
@Temperature 150 °C
696 ksi
@Temperature 302 °F
ASTM D 638
 10.0 GPa
@Temperature 23.0 °C
1450 ksi
@Temperature 73.4 °F
ISO 527
 10.5 GPa
@Temperature 23.0 °C
1520 ksi
@Temperature 73.4 °F
ASTM D 638
 11.6 GPa
@Temperature -40.0 °C
1680 ksi
@Temperature -40.0 °F
ASTM D 638
Flexural Strength 145 MPa
@Temperature 23.0 °C
21000 psi
@Temperature 73.4 °F
ISO 178
 42.0 MPa
@Thickness 3.17 mm,
Temperature 150 °C
6090 psi
@Thickness 0.125 in,
Temperature 302 °F
ASTM D790
 50.0 MPa
@Thickness 0.800 mm,
Temperature 150 °C
7250 psi
@Thickness 0.0315 in,
Temperature 302 °F
ASTM D790
 51.0 MPa
@Thickness 3.17 mm,
Temperature 120 °C
7400 psi
@Thickness 0.125 in,
Temperature 248 °F
ASTM D790
 60.0 MPa
@Thickness 0.800 mm,
Temperature 120 °C
8700 psi
@Thickness 0.0315 in,
Temperature 248 °F
ASTM D790
 127 MPa
@Thickness 3.17 mm,
Temperature 23.0 °C
18400 psi
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D790
 158 MPa
@Thickness 0.800 mm,
Temperature 23.0 °C
22900 psi
@Thickness 0.0315 in,
Temperature 73.4 °F
ASTM D790
 192 MPa
@Thickness 3.17 mm,
Temperature -40.0 °C
27800 psi
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D790
 260 MPa
@Thickness 0.800 mm,
Temperature -40.0 °C
37700 psi
@Thickness 0.0315 in,
Temperature -40.0 °F
ASTM D790
Flexural Modulus 7.10 GPa
@Temperature 23.0 °C
1030 ksi
@Temperature 73.4 °F
ISO 178
 3.30 GPa
@Thickness 3.17 mm,
Temperature 150 °C
479 ksi
@Thickness 0.125 in,
Temperature 302 °F
ASTM D790
 3.40 GPa
@Thickness 3.17 mm,
Temperature 120 °C
493 ksi
@Thickness 0.125 in,
Temperature 248 °F
ASTM D790
 5.00 GPa
@Thickness 0.800 mm,
Temperature 150 °C
725 ksi
@Thickness 0.0315 in,
Temperature 302 °F
ASTM D790
 5.16 GPa
@Thickness 0.800 mm,
Temperature 120 °C
748 ksi
@Thickness 0.0315 in,
Temperature 248 °F
ASTM D790
 9.60 GPa
@Thickness 3.17 mm,
Temperature 23.0 °C
1390 ksi
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D790
 10.7 GPa
@Thickness 3.17 mm,
Temperature -40.0 °C
1550 ksi
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D790
 13.9 GPa
@Thickness 0.800 mm,
Temperature 23.0 °C
2020 ksi
@Thickness 0.0315 in,
Temperature 73.4 °F
ASTM D790
 16.7 GPa
@Thickness 0.800 mm,
Temperature -40.0 °C
2420 ksi
@Thickness 0.0315 in,
Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 1.60 J/cm
@Temperature 23.0 °C
3.00 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D 257
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D 257
Dielectric Constant  2.9
@Frequency 1e+6 Hz,
Temperature 23.0 °C
2.9
@Frequency 1e+6 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
 3.2
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.2
@Frequency 1e+6 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 3.3
@Frequency 1000 Hz,
Temperature 23.0 °C
3.3
@Frequency 1000 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
 3.3
@Frequency 100 Hz,
Temperature 23.0 °C
3.3
@Frequency 100 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
 3.6
@Frequency 100 Hz,
Temperature 23.0 °C
3.6
@Frequency 100 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 3.6
@Frequency 1000 Hz,
Temperature 23.0 °C
3.6
@Frequency 1000 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
3.9
@Frequency 1e+9 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 2520 B
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
3.9
@Frequency 1e+9 Hz,
Temperature 73.4 °F
1.6mm (0.062in); ASTM D 2520 B
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
3.9
@Frequency 1e+9 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 23.0 °C
4.0
@Frequency 1e+10 Hz,
Temperature 73.4 °F
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 120 °C
4.0
@Frequency 1e+10 Hz,
Temperature 248 °F
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
4.0
@Frequency 1e+9 Hz,
Temperature 248 °F
0.8mm (0.031in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
4.0
@Frequency 1e+9 Hz,
Temperature 248 °F
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
4.0
@Frequency 1e+9 Hz,
Temperature 248 °F
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
4.0
@Frequency 1e+9 Hz,
Temperature 302 °F
0.8mm (0.031in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
4.0
@Frequency 1e+9 Hz,
Temperature 302 °F
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
4.0
@Frequency 1e+9 Hz,
Temperature 302 °F
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 200 °C
4.0
@Frequency 1e+10 Hz,
Temperature 392 °F
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 150 °C
4.0
@Frequency 1e+10 Hz,
Temperature 302 °F
1.6mm (0.062in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 150 °C
4.1
@Frequency 1e+10 Hz,
Temperature 302 °F
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 200 °C
4.1
@Frequency 1e+10 Hz,
Temperature 392 °F
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 150 °C
4.1
@Frequency 1e+10 Hz,
Temperature 302 °F
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 120 °C
4.1
@Frequency 1e+10 Hz,
Temperature 248 °F
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 120 °C
4.1
@Frequency 1e+10 Hz,
Temperature 248 °F
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 23.0 °C
4.1
@Frequency 1e+10 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+9 Hz,
Temperature 200 °C
4.1
@Frequency 1e+9 Hz,
Temperature 392 °F
1.6mm (0.062in); ASTM D 2520 B
 4.1
@Frequency 1e+9 Hz,
Temperature 200 °C
4.1
@Frequency 1e+9 Hz,
Temperature 392 °F
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 200 °C
4.1
@Frequency 1e+10 Hz,
Temperature 392 °F
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 23.0 °C
4.1
@Frequency 1e+10 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 2520 B
 4.2
@Frequency 1e+9 Hz,
Temperature 250 °C
4.2
@Frequency 1e+9 Hz,
Temperature 482 °F
3.2mm (0.125in); ASTM D 2520 B
 4.2
@Frequency 1e+9 Hz,
Temperature 200 °C
4.2
@Frequency 1e+9 Hz,
Temperature 392 °F
0.8mm (0.031in); ASTM D 2520 B
Dielectric Strength  26.0 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
660 kV/in
@Thickness 0.126 in,
Temperature 73.4 °F
Short time; ASTM D149
 41.0 kV/mm
@Thickness 1.60 mm,
Temperature 23.0 °C
1040 kV/in
@Thickness 0.0630 in,
Temperature 73.4 °F
Short time; ASTM D149
 49.0 kV/mm
@Thickness 0.800 mm,
Temperature 23.0 °C
1240 kV/in
@Thickness 0.0315 in,
Temperature 73.4 °F
Short time; ASTM D149
Dissipation Factor  0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
0.0010
@Frequency 1e+10 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 2520 B
 0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
0.0010
@Frequency 1e+10 Hz,
Temperature 73.4 °F
1.6mm (0.062in); ASTM D 2520 B
 0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
0.0010
@Frequency 1e+10 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
0.0020
@Frequency 1e+9 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
0.0020
@Frequency 1e+9 Hz,
Temperature 73.4 °F
1.6mm (0.062in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
0.0020
@Frequency 1e+9 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 2520 B
 0.0050
@Frequency 1e+10 Hz,
Temperature 120 °C
0.0050
@Frequency 1e+10 Hz,
Temperature 248 °F
0.8mm (0.031in); ASTM D 2520 B
 0.0060
@Frequency 1e+10 Hz,
Temperature 120 °C
0.0060
@Frequency 1e+10 Hz,
Temperature 248 °F
1.6mm (0.062in); ASTM D 2520 B
 0.0060
@Frequency 1e+10 Hz,
Temperature 120 °C
0.0060
@Frequency 1e+10 Hz,
Temperature 248 °F
3.2mm (0.125in); ASTM D 2520 B
 0.0080
@Frequency 100 Hz,
Temperature 23.0 °C
0.0080
@Frequency 100 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 0.0090
@Frequency 100 Hz,
Temperature 23.0 °C
0.0090
@Frequency 100 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
0.0090
@Frequency 1e+10 Hz,
Temperature 302 °F
0.8mm (0.031in); ASTM D 2520 B
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
0.0090
@Frequency 1e+10 Hz,
Temperature 302 °F
1.6mm (0.062in); ASTM D 2520 B
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
0.0090
@Frequency 1e+10 Hz,
Temperature 302 °F
3.2mm (0.125in); ASTM D 2520 B
 0.012
@Frequency 1e+9 Hz,
Temperature 120 °C
0.012
@Frequency 1e+9 Hz,
Temperature 248 °F
0.8mm (0.031in); ASTM D 2520 B
 0.013
@Frequency 1000 Hz,
Temperature 23.0 °C
0.013
@Frequency 1000 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 0.013
@Frequency 1000 Hz,
Temperature 23.0 °C
0.013
@Frequency 1000 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
 0.014
@Frequency 1e+9 Hz,
Temperature 120 °C
0.014
@Frequency 1e+9 Hz,
Temperature 248 °F
1.6mm (0.062in); ASTM D 2520 B
 0.014
@Frequency 1e+9 Hz,
Temperature 120 °C
0.014
@Frequency 1e+9 Hz,
Temperature 248 °F
3.2mm (0.125in); ASTM D 2520 B
 0.015
@Frequency 1e+10 Hz,
Temperature 200 °C
0.015
@Frequency 1e+10 Hz,
Temperature 392 °F
3.2mm (0.125in); ASTM D 2520 B
 0.017
@Frequency 1e+10 Hz,
Temperature 200 °C
0.017
@Frequency 1e+10 Hz,
Temperature 392 °F
0.8mm (0.031in); ASTM D 2520 B
 0.018
@Frequency 1e+10 Hz,
Temperature 200 °C
0.018
@Frequency 1e+10 Hz,
Temperature 392 °F
1.6mm (0.062in); ASTM D 2520 B
 0.018
@Frequency 1e+9 Hz,
Temperature 150 °C
0.018
@Frequency 1e+9 Hz,
Temperature 302 °F
0.8mm (0.031in); ASTM D 2520 B
 0.020
@Frequency 1e+9 Hz,
Temperature 150 °C
0.020
@Frequency 1e+9 Hz,
Temperature 302 °F
3.2mm (0.125in); ASTM D 2520 B
 0.026
@Frequency 1e+9 Hz,
Temperature 250 °C
0.026
@Frequency 1e+9 Hz,
Temperature 482 °F
3.2mm (0.125in); ASTM D 2520 B
 0.027
@Frequency 1e+9 Hz,
Temperature 200 °C
0.027
@Frequency 1e+9 Hz,
Temperature 392 °F
0.8mm (0.031in); ASTM D 2520 B
 0.028
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.028
@Frequency 1e+6 Hz,
Temperature 73.4 °F
3.2mm (0.125in); ASTM D 150
 0.029
@Frequency 1e+9 Hz,
Temperature 200 °C
0.029
@Frequency 1e+9 Hz,
Temperature 392 °F
3.2mm (0.125in); ASTM D 2520 B
 0.029
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.029
@Frequency 1e+6 Hz,
Temperature 73.4 °F
0.8mm (0.031in); ASTM D 150
Comparative Tracking Index 175 - 249 V175 - 249 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C
@Temperature 23.0 - 150 °C
4.44 µin/in-°F
@Temperature 73.4 - 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 22.0 µm/m-°C
@Temperature 23.0 - 150 °C
12.2 µin/in-°F
@Temperature 73.4 - 302 °F
ASTM E 228
Melting Point 335 °C635 °FASTM D 3418
 335 °C635 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-1/-2
 245 °C473 °FASTM D 648
Glass Transition Temp, Tg 120 °C248 °FASTM D 3418
UL RTI, Electrical  240 °C
@Thickness 1.50 mm
464 °F
@Thickness 0.0591 in
UL 746B
 240 °C
@Thickness 3.00 mm
464 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact  220 °C
@Thickness 1.50 mm
428 °F
@Thickness 0.0591 in
UL 746B
 220 °C
@Thickness 3.00 mm
428 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact  240 °C
@Thickness 1.50 mm
464 °F
@Thickness 0.0591 in
UL 746B
 240 °C
@Thickness 3.00 mm
464 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 355 °C671 °FOptimum
 350 - 360 °C662 - 680 °F
Mold Temperature 80.0 °C176 °FOptimum
 40.0 - 150 °C104 - 302 °F
Drying Temperature 150 °C302 °F
Dry Time 3 hour3 hourDehumidified Dryer
Moisture Content <= 0.010 %<= 0.010 %
 
Descriptive Properties
ColorNatural
Drying RecommendedYes
FeaturesAppearance, Pleasing Surface
 Arc Resistant
 Aromatic
 Chemical Resistance, Good
 Dimensional Stability, Good
 Flow, Good
 Heat Aging Resistance, Good
 Moisture Absorption, Low
 Platable
 Warpage, Low
FillerMineral filler
Flame Retardant - Halogen/Red Phosphorus FreeYes
FormsPellets
GenericLCP
Part Marking Code>LCP-MD30<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
ProcessingInjection Moldable
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Low Warp Resins
 Mineral Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-MD30ISO 1043
UsesAutomotive Applications
 Automotive Electronics
 Automotive, Under the Hood
 Communication Applications
 Computer Components
 Connectors
 Electrical/Electronic Applications
 Parts, Engineering
 Parts, Thin-walled
 Printer Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 7130 LCP, 30% Glass Reinforced
Celanese Zenite® 6635 BK010 LCP
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced

PHCQ540b / 89599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.