MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 2158 B/A Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a gray, two-part, high strength adhesive that chemically cures at room temperature. It has good adhesion to a variety of substrates including metals, many plastics, wood and concrete.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 250000 - 450000 cP250000 - 450000 cPBase, RVF #7 sp.
 200000 - 800000 cP200000 - 800000 cPBase, RVF #7 sp.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.40e+15 ohm-cm1.40e+15 ohm-cm
Dielectric Constant 5.6
@Frequency 1000 Hz
5.6
@Frequency 1000 Hz
Dielectric Strength 38.6 kV/mm980 kV/in
Dissipation Factor 0.019
@Frequency 1000 Hz
0.019
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  53.0 µm/m-°C
@Temperature -50.0 - 30.0 °C
29.4 µin/in-°F
@Temperature -58.0 - 86.0 °F
 135 µm/m-°C
@Temperature 70.0 - 130 °C
75.0 µin/in-°F
@Temperature 158 - 266 °F
Thermal Conductivity 0.490 W/m-K3.40 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 52.0 °C126 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min8.00 - 12.0 hourTime to Handling Strength
 10100 min168 hourFull
 
Descriptive Properties
AppearanceDark GrayAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H67-MP Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy
Epoxy Technology EPO-TEK® T6067 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H70E-4 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H67MP-GB Thermally Conductive, Electrically Insulating Epoxy

PMM34629 / 169376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.