MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Trovidur® PHT PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product characteristics:
  • Uniform physical properties
  • Continuous service temperature up to 90°C
  • High resistance to acids, lyes and salt solutions
Product applications:
  • Chemical engineering and tank building
  • Clean room and semi conductor industry
  • Ventilation technology

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³DIN EN ISO 1183-1
Water Absorption <= 0.20 %<= 0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575DIN EN ISO 868
Tensile Strength, Yield 60.0 MPa8700 psiDIN EN ISO 527
Elongation at Break 15 %15 %DIN EN ISO 527
Modulus of Elasticity 3.00 GPa435 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 80.0 µm/m-°C33.3 - 44.4 µin/in-°FDIN 53752
Thermal Conductivity 0.130 W/m-K0.902 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 90.0 °C194 °Flong term
Vicat Softening Point 107 °C225 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -10.0 °C14.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 2007NAT Rigid PVC
Colorite Polymers 2007F Rigid PVC
Colorite Polymers 2002 Rigid PVC
Axiall Suprel® SVA 9412 Rigid PVC, Molding
Axiall Suprel® SVA 9301 Rigid PVC, Molding

PROCH9367 / 233069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.