MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Electrically insulating
  • Highly flexiblized
  • Room temperature curing
  • Cryogenically serviceable down to 4K
  • High peel strength and elongation
  • Good flow properties
Product Description: Master Bond EP21TDC-2 is a two component highly flexible epoxy resin compound for high performance bonding, sealing, coating and encapsulation. It has a forgiving one to three mix ratio by weight. The system is formulated to cure fully at ambient temperature or more quickly at elevated temperatures. The optimum cure schedule is overnight at room temperature followed by 2-3 hours at 150-200°F. An unusual feature here is that the curing cycle can affect the hardness of the system. If cured only at elevated temperatures, the Shore A hardness is 50-55. If cured with the optimum cure schedule, the Shore A is 75-80. It has very high peel strength and elongation. EP21TDC-2 develops very little exotherm while curing, making it well suited for sealing or encapsulating in thicker sections. It has excellent adhesion to a wide array of substrates including metals, composites, glass, ceramics and many rubbers and plastics. Its superior flexibility allows EP21TDC-2 to have excellent thermal cycling properties along with exceptional resistance to thermal and mechanical shock and vibration. This epoxy is a superb electrical and thermal insulator with good resistance to chemicals such as water, oils, hydraulic fluids, bases and salts. EP21TDC-2 is cryogenically serviceable and has a temperature range of 4K to +250°F. EP21TDC-2 is widely used in aerospace, specialty OEM, optical and especially in applications where robust thermal cycling properties and shock resistance are paramount.

Product Advantages:

  • Easy application: good flow, product spreads evenly and smoothly
  • Cures readily at ambient temperature or faster at elevated temperatures
  • Variable hardness and flexibility depending upon cure schedule
  • Bonds well to a wide variety of substrates
  • Excellent peel strength, dependable resistance to rigorous thermal cycling
  • Cryogenic serviceability

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 10000 - 20000 cPPart A
 150000 - 300000 cPPart B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50 - 55Cured at 150-200°F
 75 - 80Cured with optimum schedule
Tensile Strength >= 5000 psi
Adhesive Bond Strength >= 1200 psiTensile lap, Aluminum to Aluminum
Peel Strength >= 30.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.6
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.4423 W/m-K
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -269 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 48.0 - 72.0 hour
@Temperature 23.9 °C
Working Life >= 60.0 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Cure ScheduleOvernight at 75°Ffollowed by 2-3 hours at 200°F, Optimum cure
Mixing Ratio1:3 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Goodfellow Niobium 56/Titanium 44 Alloy
Master Bond EP30DP Abrasion Resistant Cryogenic Epoxy Urethane System
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy
Master Bond EP37-3FLFAO Low Outgassing Thermally Conductive Epoxy System

PMASTM832 / 185425

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.