MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Grade 12, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Addition of 0.3% Mo and 0.8% Ni to titanium increases corrosion resistance at a lower cost than Pd (see Ti Grades 7 and 11). Sample was annealed 20 min. at 815°C and 5 min. at 788°C.

Higher strength than unalloyed Ti grades 1 - 4, yet still formable.

Microstructure: Equiaxed alpha, with acicular alpha, primarily in welds or heat-affected zones, small amounts of beta.

Applications: Chemical processing, in mildly reducing or variable oxidizing-reducing media - containers, heat exchangers, pumps, valves, pipes and fittings.

Forms typically available: billet, bar, rod, plate, sheet, strip and tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: UNS R53400; ASTM Grade 12, titanium alloy
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 345 MPa
@Temperature 316 °C
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 480 MPa
Elongation at Break 23 %
Creep Strength 103 MPa
@Temperature 316 °C,
Time >=3.60e+6 sec
strain 0.3%
Rupture Strength 276 MPa
@Temperature 316 °C,
Time 3.60e+6 sec
Tensile Modulus 103 GPa
Modulus of Rigidity 41.3 GPa
Notched Tensile Strength 620 MPaKt (stress concentration factor) = 5.3
Poissons Ratio 0.28
Fatigue Strength 140 MPa
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 3.5
 310 MPa
@# of Cycles 1.00e+7
unnotched
Shear Modulus 41.0 GPa
Bend Radius, Minimum 2.5 t
@Thickness >=1.80 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000520 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/gHigh Purity Ti.
CTE, linear 9.50 µm/m-°C
@Temperature 200 °C
 9.90 µm/m-°C
@Temperature 20.0 - 93.0 °C
 19.9 µm/m-°C
@Temperature 20.0 °C
perpendicular
Specific Heat Capacity 0.555 J/g-°C
Thermal Conductivity 19.0 W/m-K
Melting Point <= 1660 °C
Liquidus 1660 °C
Beta Transus 890 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 710 °C
High purity Ti
Reflection Coefficient, Visible (0-1) 0.56High purity Ti; visible light.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.30 %
Molybdenum, Mo 0.20 - 0.40 %
Nickel, Ni 0.60 - 0.90 %
Nitrogen, N <= 0.030 %
Other, each <= 0.050 %
Other, total <= 0.30 %
Oxygen, O <= 0.25 %
Titanium, Ti 97.725 - 99.2 %As Balance; Elemental Composition per ASTM B265

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 12
Titanium Grade 1
Titanium Grade 1, Annealed
Titanium Grade 2, Annealed
Titanium Grade 7

MTU121 / 14269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.