MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum 2218-T71
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2218-T72; UNS A92218; AMS 4142; NF A-U4N (France); QQ-A-367; SAE J454; AA2218-T72; Al2218-T71
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.81 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105500 kg load with 10 mm ball
Hardness, Knoop 132Converted from Brinell Hardness Value
Hardness, Rockwell A 43Converted from Brinell Hardness Value
Hardness, Rockwell B 66Converted from Brinell Hardness Value
Hardness, Vickers 118Converted from Brinell Hardness Value
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 280 MPa
Elongation at Break 11 %In 5 cm; Sample 1.6 mm thick
Modulus of Elasticity 74.4 GPaAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.33
Shear Modulus 27.5 GPa
Shear Strength 207 MPaCalculated value.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000430 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 20.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
 22.4 µm/m-°C
@Temperature 20.0 - 100 °C
 23.3 µm/m-°C
@Temperature 20.0 - 200 °C
 24.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Thermal Conductivity 155 W/m-K
Melting Point 935 - 1180 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
Solidus 935 °FAA; Typical
Liquidus 1180 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Solution Temperature 950 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.8 - 93.6 %As remainder
Chromium, Cr <= 0.10 %
Copper, Cu 3.5 - 4.5 %
Iron, Fe <= 1.0 %
Magnesium, Mg 1.2 - 1.8 %
Manganese, Mn <= 0.20 %
Nickel, Ni 1.7 - 2.3 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.90 %
Zinc, Zn <= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2124-T851
Aluminum 2218-T72
Aluminum 2219-T31
Aluminum 2124-O
Aluminum 2124-T351

MA2218T71 / 8924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.