MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 7050-T7451 (7050-T73651)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: 7050 has very high strength coupled with high resistance to exfoliation corrosion and stress-corrosion cracking, high fracture toughness, and fatigue resistance. This leads to applications in aircraft structures.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: AA7050-T7451; AA7070-T73651, UNS A97050; ISO AlZn6CuMgZr; Aluminium 7050-T7451; Aluminium 7070-T73651; Al7050-T7451
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.83 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 140500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 177Converted from Brinell Hardness Value
Hardness, Rockwell A 51.6Converted from Brinell Hardness Value
Hardness, Rockwell B 84Converted from Brinell Hardness Value
Hardness, Vickers 162Converted from Brinell Hardness Value
Tensile Strength, Ultimate 76.0 ksiAA; Typical
Tensile Strength, Yield 68.0 ksiAA; Typical
Elongation at Break 11 %
@Diameter 12.7 mm
AA; Typical
Modulus of Elasticity 10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.33
Fracture Toughness >= 22.0 MPa-m½S-L
 >= 24.2 MPa-m½T-L
 >= 26.4 MPa-m½L-T
 28.0 MPa-m½K(IC) in S-L Direction
 28.6 MPa-m½average; S-L
 29.7 MPa-m½average; T-L
 31.0 MPa-m½K(IC) in T-L Direction
 35.0 MPa-m½K(IC) in L-T Direction
 35.2 MPa-m½average; L-T
Shear Modulus 26.9 GPa
Shear Strength 44.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000430 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.8 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.860 J/g-°C
Thermal Conductivity 157 W/m-K
Melting Point 910 - 1165 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 910 °FAA; Typical
Liquidus 1165 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 775 °F
Solution Temperature 890 °F
Aging Temperature 250 - 350 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87.3 - 90.3 %As remainder
Chromium, Cr <= 0.04 %
Copper, Cu 2.0 - 2.6 %
Iron, Fe <= 0.15 %
Magnesium, Mg 1.9 - 2.6 %
Manganese, Mn <= 0.10 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.12 %
Titanium, Ti <= 0.06 %
Zinc, Zn 5.7 - 6.7 %
Zirconium, Zr 0.08 - 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 7050-T7651
Aluminum 7050-T73511; 7050-T73510
Aluminum 7050-T74
Aluminum 7050-T73651 plate

MA7050T745 / 9577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.