MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
European Beech Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Excellent bending properties. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Resistance to penetration by preservatives: Regular
Common Applications: Furniture, interior joinery, flooring. Plywood

Key Words: Fagus sylvatica; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.660 - 0.780 g/cc
Cell Length 1.10 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4800 NSide
Tensile Strength, Ultimate 3.50 MPaPerpendicular to Grain
 130 MPaAxial
Modulus of Rupture 0.104 GPaStatic Bending
Flexural Modulus 13.13 GPaStatic Bending
Compressive Strength 7.90 MPaPerpendicular to Grain
 46.0 MPaParallel to Grain
Machinability 100 %Good Relative to Other Wood
Shear Strength 12.3 MPaOrientation Unknown
Toughness 31.2 J2 cm x 2 cm sample
Cleavage 9.10 kN/m
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.10 - 1.1 %Axial; Green to Zero Moisture
 5.8 %Nominal; Radial; Green to Zero Moisture
 3.0 - 9.8 %Radial; Green to Zero Moisture
 8.6 - 18.2 %Tangential; Green to Zero Moisture
 12.3 - 21.8 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorPinkish-redSteamed; Usual for heartwood
 Whitish to pale brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
European Birch Wood
American Beech Wood
American White Ash Wood
Aluminum, Al
American White Oak Wood

PTSE030 / 71312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.