MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 152 Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Superb flexibility
  • Outstanding optical clarity
  • Highly electrically insulative
  • Service temperature is -65°F to +400°F
  • Very low viscosity
  • Cures at room temperatures
Product Description: Master Bond MasterSil 152 is a two component, very low viscosity silicone for high performance bonding and encapsulation. It is a condensation curing system and after mixing, it only requires air for complete crosslinking. Curing is at room temperature only, with a full cure in 24-48 hours. The mix ratio is ten to one by weight and the system contains no solvents or diluents. With its exceptionally low viscosity, MasterSil 152 is ideal for potting and encapsulation. It combines high temperature resistance, marvelous flexibility, top notch electrical insulation values and wonderful optical clarity. It is capable of withstanding the most rigorous thermal cycling and shock. Its water resistance is quite good. These properties enable MasterSil 152 to be used in applications involving sensitive optical and electrical components. Some other specialty uses include encapsulating LEDs, optical fiber cladding and potting connectors. Its index of refraction is 1.45 and it can transmit light very well from 220-2,500 nanometers. The service temperature range for this system is -65°F to +400°F. Unlike addition cured systems, there are no substrates that will inhibit the cure. MasterSil 152 has prominence in optical, opto-electronic, specialty OEM and related applications primarily in situations where the addition cured silicone cannot be used.

Product Advantages:

  • Requires only the presence of air for curing; no substrate inhibition
  • Low exotherm; very long pot life
  • Will cure in thicker sections (>1 inch)
  • Low shrinkage upon cure
  • Very low viscosity ideal for potting and encapsulation
  • Excellent optical clarity and transmission properties
  • Lower index of refraction
  • Superior electrical insulation properties; highly resistant to water

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 50 - 150 cPPart B
 500 - 900 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25 - 35
Tensile Strength 100 - 150 psi
Elongation at Break 150 - 180 %
Adhesive Bond Strength >= 35.0 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 2.4
@Frequency 60 Hz
Dielectric Strength 450 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -65.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.45
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 48.0 hour
@Temperature 23.9 °C
must be exposed air
Working Life 360 - 480 min100 g. batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio10:1 by weightPart A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy
Master Bond EP38FLAO Two Component Epoxy
Master Bond EP90FR-HFL Two Component Epoxy
Master Bond MasterSil 151AN Silicone Features High Thermal Conductivity
Henkel Loctite® Nuva-Sil® 5088 Potting Compound

PMASTM930 / 185523

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.