MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depths. Typical uses: Low viscosity, clear uses.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Viscosity 1000 cP
@Temperature 25.0 °C
1000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength, Ultimate 0.980 MPa142 psi
Elongation at Break 130 %130 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 2.8
@Frequency 1000 Hz
2.8
@Frequency 1000 Hz
Dielectric Strength 21.0 kV/mm
@Thickness 1.91 mm
533 kV/in
@Thickness 0.0750 in
Dissipation Factor 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 230 µm/m-°C
@Temperature 20.0 °C
128 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °FContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °C-76.0 °FContinuous useful temperature.
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4061.406
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCure time 6 hours.
Pot Life 360 min
@Temperature 25.0 °C
360 min
@Temperature 77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 415 One Component Room Temperature Curing, Transparent Silicon
Lord Adhesives Thermoset™ SC-300M Silicone Gel Encapsulant
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin
Renishaw 6230 Vacuum casting resin
Celanese Riteflex® 663 TPC, Unfilled

PZZGE986 / 40540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.