MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Bronze, UNS C95500 Casting Alloy, TQ50 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: High strength, heat treatable.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Valve guides and seats in aircraft engines, corrosion-resistant parts, bushings, gears, worms, pickling hooks and baskets, agitators.

ASTM B148; formerly ASTM B148-9D.

Tempering: Solution treated at 855°C (1575°F), quenched, tempered 2 hours at 650°C (1200°F).

Key Words: Nickel aluminum bronze, ASTM B148, ASTM B148-9D
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217 - 234217 - 2343000 kg load
Hardness, Rockwell B 9696
Tensile Strength, Ultimate 760 - 800 MPa110000 - 116000 psi
Tensile Strength, Yield 415 - 470 MPa60200 - 68200 psi
Elongation at Break 5.0 - 14 %5.0 - 14 %in 50 mm
Reduction of Area 5.0 %5.0 %
Creep Strength  17.0 MPa
@Temperature 425 °C
2470 psi
@Temperature 797 °F
for 0.00001%/h
 38.0 MPa
@Temperature 370 °C
5510 psi
@Temperature 698 °F
for 0.00001%/h
 72.0 MPa
@Temperature 315 °C
10400 psi
@Temperature 599 °F
for 0.00001%/h
Modulus of Elasticity 115 GPa16700 ksi
Compressive Yield Strength 1030 MPa149000 psiat permanent set of 10%
Compressive Strength 1140 MPa165000 psi
Poissons Ratio 0.320.32
Fatigue Strength 260 MPa
@# of Cycles 1.00e+8
37700 psi
@# of Cycles 1.00e+8
rotating beam
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.0 GPa6090 ksi
Shear Strength 44.0 MPa6380 psi
Izod Impact 18.0 J
@Temperature 20.0 °C
13.3 ft-lb
@Temperature 68.0 °F
Charpy Impact 14.0 J10.3 ft-lbKeyhole
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000203 ohm-cm
@Temperature 20.0 °C
0.0000203 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.21.216 kA/m field strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.418 J/g-°C0.0999 BTU/lb-°F
Thermal Conductivity 42.0 W/m-K
@Temperature 20.0 °C
291 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1055 °C1900 - 1931 °F
Solidus 1040 °C1900 °F
Liquidus 1055 °C1931 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 620 - 705 °C1150 - 1300 °F
Solution Temperature 855 °C1570 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10 - 11.5 %10 - 11.5 %
Copper, Cu >= 78 %>= 78 %
Iron, Fe 3.0 - 5.0 %3.0 - 5.0 %
Manganese, Mn <= 3.5 %<= 3.5 %
Nickel, Ni 3.0 - 5.5 %3.0 - 5.5 %
Other, total <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
MetalTek MTEK 230 Cast UNS C95500 Aluminum Bronze
Aluminum Bronze, UNS C95200, Copper Casting Alloy
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze
Aluminum 7050-T73651 plate

MC95410b3 / 193496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.