MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum Bronze, UNS C95500 Casting Alloy, TQ50 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: High strength, heat treatable.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Valve guides and seats in aircraft engines, corrosion-resistant parts, bushings, gears, worms, pickling hooks and baskets, agitators.

ASTM B148; formerly ASTM B148-9D.

Tempering: Solution treated at 855°C (1575°F), quenched, tempered 2 hours at 650°C (1200°F).

Key Words: Nickel aluminum bronze, ASTM B148, ASTM B148-9D
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217 - 2343000 kg load
Hardness, Rockwell B 96
Tensile Strength, Ultimate 760 - 800 MPa
Tensile Strength, Yield 415 - 470 MPa
Elongation at Break 5.0 - 14 %in 50 mm
Reduction of Area 5.0 %
Creep Strength 17.0 MPa
@Temperature 425 °C
for 0.00001%/h
 38.0 MPa
@Temperature 370 °C
for 0.00001%/h
 72.0 MPa
@Temperature 315 °C
for 0.00001%/h
Modulus of Elasticity 115 GPa
Compressive Yield Strength 1030 MPaat permanent set of 10%
Compressive Strength 1140 MPa
Poissons Ratio 0.32
Fatigue Strength 260 MPa
@# of Cycles 1.00e+8
rotating beam
Machinability 50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.0 GPa
Shear Strength 44.0 MPa
Izod Impact 18.0 J
@Temperature 20.0 °C
Charpy Impact 14.0 JKeyhole
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000203 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.216 kA/m field strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.418 J/g-°C
Thermal Conductivity 42.0 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1055 °C
Solidus 1040 °C
Liquidus 1055 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 620 - 705 °C
Solution Temperature 855 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10 - 11.5 %
Copper, Cu >= 78 %
Iron, Fe 3.0 - 5.0 %
Manganese, Mn <= 3.5 %
Nickel, Ni 3.0 - 5.5 %
Other, total <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
MetalTek MTEK 230 Cast UNS C95500 Aluminum Bronze
Aluminum Bronze, UNS C95200, Copper Casting Alloy
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze
Aluminum 7050-T73651 plate

MC95410b3 / 193496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.